NEXTERION® coated glass substrates
With NEXTERION®, SCHOTT MINIFAB offers functional coating chemistries for DNA and protein microarrays and a wide range of other applications to meet your exact needs. Find out more about the coating that fits your challenge.
Epoxysilane coating (E)
Product information
These substrates have a multi-purpose epoxysilane layer that will covalently bind most types of bio-molecules including amino- and non-modified DNA, RNA, and proteins.
The defect-free surface features a uniform epoxysilane layer that provides a high covalent coupling efficiency together with a very low background. The robust and stable surface chemistry easily allows long print runs. This type of substrate is easy to use and protocols for many applications are published in literature.
Produced in ISO class 5 clean room conditions using a standardized process and running a stringent quality control system, epoxysilane coated substrates are available in standard and custom formats.
Probe types
- Amino-modified oligonucleotides (necessary for < 20 mers)
- Unmodified oligonucleotides
- PCR products
- ZIP code oligonucleotides
- BACs, PACs, YACs, plasmids
- L-DNA, cDBA, RNA
- Serum samples
- Proteins, Antibodies, Peptides, Glucans
Shelf life
Twelve months for sealed packages at room temperature.
Immobilization method
Covalent binding via amino-, thiol- and hydroxyl-reactive chemistry.
3-D Hydrogel coating
Product information
This type of coating has proven to be a very attractive alternative to the commonly used nitrocellulose-coated slides, especially when low background noise or slide transparency are important. It ensures an extremely low non-specific binding and helps preserving the native three-dimensional structure of complex bio-molecules, thus maintaining conformation and functionality. As a result, it attains excellent signal-to-background ratios.
Produced in ISO class 5 clean room conditions using a proprietary thin-film deposition process and running a stringent quality control system, the 3-D hydrogel coating is offered in standard and custom formats.
Probe types
- Amino-linked glucans
- Antibodies and antibody fragments
- Functional proteins such as enzymes or receptors
- Small protein fragments such as peptides
- Amino-modified oligonucleotides 16 to 70 mers
Shelf life
Twelve months sealed packages when stored at - 20° C.
Immobilization method
Covalent binding via amine reactive chemistry.Aminosilane coating (A+)
Product information
The coating is based on very short chains of aminosilanes that demonstrate high signal intensities and exceptionally low background noise signals in comparison to other commercially available aminosilane coated substrates. Produced in ISO class 5 clean room conditions using a standardized process and running a stringent quality control system, aminosilane coated substrates are available in standard and custom formats.
Probe types
- BACs, PACs, YACs
- Oligonucleotides ≥ 40 mers
- cDNA
- PCR products
Shelf life
Nine months for sealed packages at room temperature
Immobilization method
Ionic interaction followed by cross-linking via an additional UV or baking st
Streptavidin coating (HS)
Product information
The proprietary thin-film deposition coating process produces a very high density, as well as an extremely uniform coating of streptavidin molecules. The resulting surface has a very high binding capacity combined with a low signal variance across a single slide as well as different slides and batches.
Produced in ISO class 5 clean room conditions using a standardized process and running a stringent quality control system, streptavidin coated substrates are available in standard and custom formats
Shelf life
Six months for sealed packages when stored at – 20° C.
To protect the activity of the streptavidin layer, a protective coating is added on top of the reactive coating prior to packaging. This layer must be removed prior to use by a washing step. The streptavidin layer on Slide HS is very sensitive to elevated temperatures. It is therefore necessary to ship the product in a frozen state with dry ice. The product must immediately be put into a freezer upon arrival. Repeated freeze and thaw cycles should be avoided.
Probe types
-
All molecules that can be biotinylated
Immobilization method
Binding via biotin
Poly-L-Lysine coating (PLL)
Product information
This coating is based on long chains of positively charged L-lysin polymers. Produced in ISO class 5 clean room conditions using a standardized process following a stringent quality control system, NEXTERION® poly-L-lysine coated substrates are available in both standard and custom formats.Probe types
- BACs, PACs, YACs
- Oligonucleotides ≥ 40 mers
- cDNA
- PCR products
Shelf life
Six months for sealed packages at room temperature.
Immobilization method
Ionic interactions
Aldehydesilane coating (AL)
Product information
The covalent bond formed at the terminus of the nucleic acid offers both: stability and maximal base pairing opportunity. The covalent binding diminishes sample loss during the course of experiments and permits stringent washing steps, which reduce background noise and allow greater sensitivity. Additional immobilization steps, such as baking or UV cross-linking, are not required for immobilization.
Produced in ISO class 5 clean room conditions using a standardized process and running a stringent quality control system, aldehydesilane coated substrates are available in standard and custom formats.
Probe types
- Amino-modified PCR products and BACs/YACs
- Amino-modified oligonucleotides
- Small protein fragments such as peptides
Shelf life
Nine months for sealed packages at room temperature
Immobilization method
Covalent binding via amine reactive chemistry.
3-D Polymer coating (P)
Product information
SCHOTT specifically developed the 3-D Polymer coating as a dedicated substrate surface for printing low-density antibody microarrays. It produces excellent signal-to-background ratios, and exceptionally wide dynamic ranges compared to conventional “two-dimensional” coatings through a unique combination of low non-specific binding characteristics, and high probe loading capacity.
Produced in ISO class 5 clean room conditions using a pro-prietary thin-film deposition process and running a stringent quality control system, the 3-D Polymer coating is offered in standard and custom formats.
Probe types
-
Amino-linked glucans
-
Antibodies and antibody fragments
-
Functional proteins such as enzymes or receptors
-
Small protein fragments such as peptides
-
Amino-modified oligonucleotides 16 to 70 mers
Shelf life
Twelve months sealed packages when stored at - 20° C.
Immobilization method
Covalent binding via amine reactive chemistry.
SCHOTT MINIFAB also offers microarray printing expertise.
Want to know more? Let's talk
Whether you need more information, samples, a quote, or advice for a project, I would be delighted to talk to you.
Preview environment - pls. be aware that this page only displays the staged content and is not functional!