D 263® M
CHARACTERISTICS
D 263® M cover glass has a chemical composition that ensures valid and reliable research results. This is due to low autofluoresence and high chemical resistance, as well as a refractive index finely tuned to microscopy use. With standard thicknesses from 0.1 mm to 0.21 mm, it’s also available from stock in a wide variety of easy-to-cut sheet sizes.
YOUR ADVANTAGES
- Conforms to industry standard ISO 8255-1.
- Various sheet sizes and thicknesses from 0.1 mm to 0.21 mm available, plus custom shapes and sizes upon request.
- An industry-leading cover glass in the microscopy field.
- Outstanding geometrical properties including tight tolerances and excellent optical performance.