Xensation®
Technical excellence for maximum cover glass protection and durability
Mechanical properties
Description |
Xensation® α |
Xensation® Up. |
---|---|---|
Density ρ |
2.39 g/cm3 |
2.48 g/cm3 |
Young’s modulus E |
80 kN/mm2 |
82 kN/mm2 |
Poisson’s ratio ν |
0.26 |
0.22 |
Shear modulus G |
32 kN/mm2 |
34 kN/mm2 |
Vickers hardness HV |
|
|
> unstrengthened |
570 |
630 |
> strengthened* |
660 |
680 |
Thermal properties
Description |
Xensation® α |
Xensation® Up. |
---|---|---|
Coefficient of mean linear thermal expansion α(20 – 300 °C) |
5.3 · 10 –6 K–1 |
8.3 · 10 –6 K–1 |
Transformation temperature Tg |
577 °C |
525 °C |
Viscosity |
|
|
> Annealing point at 1013 dPas |
589 °C |
540 °C |
> Softening point at 107.6 dPas |
840 °C |
760 °C |
> Working point at 104 dPas | 1233 °C | 1120 °C |
Optical properties
Description | Xensation® α | Xensation® Up. | ||||||||
---|---|---|---|---|---|---|---|---|---|---|
Wavelength λ [nm] | 365 | 405 | 518 | 595 | 640 | 365 | 405 | 518 | 595 | 640 |
Measurement method | FSM-UV | SLP-2000 | SLP-2000 | FSM-LE | SLP-1000 | FSM-UV | SLP-2000 | SLP-2000 | FSM-LE | SLP-1000 |
Refractive index n of core glass | 1.528 | 1.522 | 1.512 | 1.508 | 1.507 | 1.546 | 1.537 | 1.525 | 1.521 | 1.520 |
Refractive index n of K-exchanged layer* | 1.531 | 1.525 | 1.514 | 1.510 | 1.508 | 1.554 | 1.542 | 1.528 | 1.523 | 1.522 |
Photoelastic constant C [nm/(cm*MPa)] | 32.3 | 31.6 | 30.5 | 30.0 | 29.08 | 30.2 | 29.0 | 28.2 | 27.08 | 27.06 |
Transmittance T [%] (t = 0.78 mm) | 89 | 90 | 91 | 91 | 92 | 89 | 90 | 90 | 91 | 92 |
Chemical properties
Description |
Xensation® α |
Xensation® Up. |
---|---|---|
Hydrolytic resistance acc. to DIN ISO 719 |
|
|
> Hydrolytic class |
HGB1 |
HGB2 |
> Equivalent of alkali Na2O per gram of glass grains [µg/g] | 32 | 38 |
Acid resistance acc. to DIN 12 116 |
|
|
> Acid class |
S2 |
S4 |
> Half surface weight loss after 6 hours [mg/dm²] |
1.4 |
19 |
Alkali resistance acc. to DIN ISO 695 | ||
> Alkali class | A2 | A1 |
> Surface weight loss after 3 hours [mg/dm²] | 92 | 42 |
Electrical properties (extrapolated)
Xensation® α | Xensation® Up. | |||
---|---|---|---|---|
Frequency ƒ0 [MHz] | Dielectric constant ε | Loss tangent tan δ | Dielectric constant ε | Loss tangent tan δ |
54 | 6.1 | 0.008 | 7.3 | 0.007 |
480 | 6.0 | 0.009 | 7.1 | 0.008 |
825 | 6.0 | 0.010 | 7.1 | 0.009 |
912 | 6.0 | 0.010 | 7.1 | 0.009 |
1977 | 6.0 | 0.011 | 7.0 | 0.010 |
2170 | 6.0 | 0.011 | 7.0 | 0.010 |
2986 | 6.0 | 0.012 | 7.0 | 0.011 |
Chemical strengthening*
Description |
Xensation® α |
Xensation® Up. |
---|---|---|
Compressive stress CS |
capable > 900 MPa |
capable > 900 MPa |
Depth of compressive layer DoCL |
capable > 180 µm |
capable > 150 µm |
4-Point bending strength |
capable > 800 MPa |
capable > 700 MPa |
* Values that can be achieved after chemical strengthening process
Forms supplied**
Description |
Xensation® α |
Xensation® Up. |
---|---|---|
Thickness range |
0.55 – 0.80 mm |
0.55 – 0.80 mm |
Sheet size |
1150 mm x 950 mm |
1150 mm x 950 mm |
** Further thicknesses and sheet sizes are available on request
All values are typical measured values and refer to unstrengthened glass.