Passivation Glass

A vast selection of compositions – including lead-free options – means that SCHOTT Passivation Glass can be precisely matched with a diverse range of electrical components. Customers benefit from impressive insulation resistance thanks to our expert selection and processing of high-quality materials.

Finely tuned compositions for excellent component matching

Excellent insulation resistance

SCHOTT achieves high insulation resistance for its passivation glass powder by using material with very low alkali content, especially from sodium. This is achieved by sourcing the finest raw materials and using specialist production processes.

Thermal expansion matching

Our choice of compositions enables the glass’s coefficient of thermal expansion to perfectly match the semiconductor components. Varying compositions feature combinations of zinc, lead, silicate, and borate, while lead-free powders can also contain bismuth.

Lead-free glass types

SCHOTT Passivation Glasses can be offered as lead-free solutions for all common passivation applications.

Broad choice of high-quality glasses

Large assortment of high-purity glass types with standard particle size distributions and grain sizes as well as custom-made passivation glass formulations available.

Specifications

Passivation glasses are offered in a variety of individual specifications due to diversified glass systems. All passivation glasses are supplied as glass powder and available in different grain sizes.

 

SCHOTT Passivation Glasses

Technology

Passivation glass powders are manufactured in two steps:

  1. The raw glass is first melted in specially designed aggregates.
  2. The glass ribbons are ground into fine powders of different grain size distribution.

Customers process our passivation glass powders in different ways. For the manufacturing of sintered glass diodes, a slurry of glass powder and deionized water is applied to the diode body before sintering it in a furnace. For wafer passivation, an organic suspension is applied by spinning, doctor blading, sedimentation, electrophoresis, or screen printing.

Want to know more? Let's talk

Whether you need more information, samples, a quote, or advice for a project, I would be delighted to talk to you.

Lépjen kapcsolatba velünk
Antonio Trizzino

Sales Manager Europe

!

Preview environment - pls. be aware that this page only displays the staged content and is not functional!