Sheets
Down-drawn sheets
CHARACTERISTICS
The down-draw process produces thin and ultra-clear flat glasses. The process involves a ribbon of molten glass being pulled down from above before moving across various drums and through a cooling track. This results in a pristine surface that can accommodate processes such as coating, bonding and etching, with very tight thickness tolerances of ± 10µm, and a TTV < 10µm.
YOUR ADVANTAGES
- Extremely flat and smooth surface on both sides.
- Very low bulk and cosmetic defects.
- Wide thickness from direct hot forming, without the need for polishing or thinning.
- Very tight thickness tolerances to accommodate different processing methods.
- Outstanding chemical strengthening performance.
Up-drawn sheets
CHARACTERISTICS
The groundbreaking up-draw process was perfected by SCHOTT to manufacture thin and ultra-clear flat glasses. The technique involves a ribbon of molten glass being pulled up across various drums and then through a cooling track, resulting in a fire-polished surface with an outstanding surface roughness of < 0.5nm. With a thickness spectrum ranging from 0.9 mm to 10 mm, this process can be used to create supremely clear ‘ultra-white’ glass sheets.
YOUR ADVANTAGES
- Pristine fire-polished surface on both sides, with no need for further polishing.
- Defined initial thickness resulting in minimal material loss during processing.
- Enables high quality production of unique glass materials unsuited to float processing.
Floated sheets
CHARACTERISTICS
Floated glass sheets such as SCHOTT’s renowned BOROFLOAT® are created using a sophisticated process in which a continuous strip of molten glass is guided over a bath of molten tin. The glass ‘floats’ over the tin and cools to form a very flat surface on both sides of the glass, with the top fire-polished due to the effect of hot gases. The resulting sheets have a very high chemical stability, outstanding thermal resistance and strong transparency, while being mechanically robust and resistant to scratching and abrasion. The hot forming process also enables a broad thickness range.
YOUR ADVANTAGES
- Outstanding transparency and optical qualities.
- Very high thermal shock resistance, so suitable for tough environments.
- Excellent mechanical strength and resistance to damage.
- Highly homogenous material ensuring reliable performance.
- Available in a wide range of thicknesses.
Preview environment - pls. be aware that this page only displays the staged content and is not functional!