MEMpax®
High durability in extremely low thicknesses
Material properties
1. Optical properties
Optical Properties | Value |
---|---|
Refractive index* ng | 1.4803 |
Refractive index* nF' | 1.4768 |
Refractive index* nF | 1.4765 |
Refractive index* ne | 1.4732 |
Refractive index* nd | 1.4715 |
Refractive index* nD | 1.4714 |
Refractive index* nC' | 1.4696 |
Refractive index* nC | 1.4693 |
Abbe value νe | 65.4 |
Photoelastic constant in (nm/cm)/Mpa | 39.8 |
* Refractive indices: Pretreatment of samples.
Condition as supplied ["as drawn"]
2. Thermal properties
General thermal properties | Unit | Value |
---|---|---|
CTE (Coefficient of thermal expansion) α | 10-6·K-1 (20 °C; 300 °C) | 3.26 |
Mean specific heat capacity cp | in J/(g·K)(20 °C; 100 °C) | 0.82 |
Transformation temperature Tg | in °C | 532 |
Viscosities | Viscosity lg ŋ in dPas | Temperature in °C |
---|---|---|
Strain point | 14.5 | 528 |
Annealing point | 13.0 | 570 |
Softening point | 7.6 | 831 |
3. Mechanical properties
Mechanical Properties |
Unit | Value |
---|---|---|
Density ρ | in g/cm³ | 2.22 |
Young's modulus E | in kN/mm² | 62.7 |
Poisson's ratio µ | 0.196 | |
Torsion modulus G | in kN/mm² | 26.2 |
Knoop hardness | HK 0.1/20 | 430 |
Vickers hardness | HV 0.2/25 | 510 |
Chemical toughening (for thickness = 0.2 mm)
Unit |
Value |
---|---|
Temperature ϑ in °C | 430 |
Time t in h | 4 |
Compressive stress (CS) in MPa | 120 |
Depth of layer (DoL) in µm | 8 |
4. Chemical properties
Hydrolytic resistance (acc. to DIN ISO 719) | Value |
---|---|
Class | HGB 1 |
Equivalent of alkali per gram glass grains in µg/g | < 31 |
Acid resistance (acc. to DIN 12116) | Value |
---|---|
Class | S 1 |
Half surface weight loss after 6 hours in mg/dm² | 0.16 |
Alkali resistance (acc. to DIN ISO 695) | Value |
---|---|
Class | A 2 |
Surface weight loss after 3 hours in mg/dm² | 132 |
5. Electrical properties
Dielectric constant εr (at ϑ = 25 °C) | Value |
---|---|
at 1 MHz | 4.8 |
at 1 GHz | 4.4 |
at 2 GHz | 4.5 |
at 5 GHz | 4.4 |
at 24 GHz | 4.4 |
at 77 GHz | 4.4 |
Dissipation factor tan δ (at ϑ = 25 °C) |
Value |
---|---|
at 1 MHz | 38 · 10-4 |
at 1 GHz | 58 · 10-4 |
at 2 GHz | 62 · 10-4 |
at 5 GHz | 73 · 10-4 |
at 24 GHz | 100 · 10-4 |
at 77 GHz | 150 · 10-4 |
Electric volume resistivity ρD in Ω·cm direct current |
---|
1.18 ·108 ( ϑ = 250 °C) |
4.24 ·106 (ϑ = 350 °C) |
6. Transmittance values
Spectral transmittance (250 - 3150 nm)
Spectral transmittance (250 - 500 nm)
Wavelength in nm at thickness 0.2 mm: | τ (λ) in % |
---|---|
254 | 28 |
380 | 92.4 |
632.8 | 92.8 |
1064 | 92.7 |
Edge wavelength λc (τ = 0.46) at thickness in mm | Wavelength in nm |
---|---|
0.2 | 269 |
0.3 | 279 |
0.5 | 283 |
0.7 | 288 |
Luminous transmittance at thickness in mm | τvD65in % |
---|---|
0.2 | 92.8 |
0.5 | 92.8 |
MEMpax® products
SCHOTT MEMpax® is available as:
- Unpolished substrates and wafers