SCHOTT® low-loss
Excellent dielectric properties for radio-frequency communication and sensing applications
General Properties | |
---|---|
Density ρ [g/cm³] | 2.14 |
Thermal properties | |
---|---|
Thermal expansion coefficient α [10-6 K-1] | 3.29 |
Thermal conductivity λ(25 °C) [W/(m·K)] | t.b.d. |
Specific heat capacity Cp(20 °C; 100 °C) [J/K] |
t.b.d. |
Transformation temperature Tg [°C] | 467 |
Strain point at 1014.5 dPas [°C] | 548 |
Annealing point at 1013 dPas [°C] |
538 |
Softening point at 107.6 dPas [°C] |
750 |
Working point at 104 dPas [°C] |
1143 |
Electrical properties |
||
---|---|---|
Frequency f [GHz] |
Dielectric constant ε ± 0.1 / measured |
Tangent delta tan δ ± 0.0005 / measured |
1 | 4.05 | 0.0011 |
2 | 4.05 |
0.0013 |
2.45 | 4.05 |
0.0014 |
5 | 4.05 | 0.0017 |
10 | 4.05 | 0.0021 |
15 | 4.05 |
0.0024 |
24 | 4.05 |
0.0028 |
77 | 4.05 |
0.0047 |
110 | 4.05 |
0.0061 |
Log10 Electric volume resistivity ρ [Ω·cm] | ||
T = 250 °C | 10.7 |
|
T = 350 °C |
8.8 |
|
TK100 [°C] |
405 |
Mechanical Properties | |
---|---|
Young’s Modulus E [GPa] | 51 |
Poisson’s ratio ν | 0.223 |
Shear Modulus G [GPa] |
21 |
Vicker Hardness [HV] |
t.b.d. |
Martens Hardness [HM] |
t.b.d. |
Knoop Hardness |
t.b.d. |
Optical properties | |
---|---|
Photo-elastic constant C [nm/(cm MPa)] | t.b.d. |
Transmittance | t.b.d. |
Chemical durability of raw glass | |
---|---|
Hydrolytic resistance acc. to DIN ISO 719 | |
Hydrolytic Class | HGB 1 |
Acid resistance acc. to DIN 12116 |
|
Acid class |
S1W |
Alkali resistance acc. to DIN ISO 695 |
|
Alkali class |
A3 |
Refractive Index