FOTURAN® II
Homogenous, versatile and precise
Available products
SCHOTT FOTURAN® II is available as:
- Polished substrates and wafers
To find out more, please see the related products on the overview page.
Structuring process and characteristics
Working principle
FOTURAN® II is a photo-structurable glass-ceramic and structured in three steps – Ceramization as a 4th step is optional
1) Different temperature profiles during crystallization lead to different crystal structures
Standard photostructuring process
FOTURAN® II structuring consists of UV exposure, heat-treatment and etching - subsequent ceramization is optional
1) For 0.5 mm thick substrates – Parameter for other thicknesses may differ
2) Optimal theoretical exposure wavelength is 312 nm
Transmission curve of unprocessed FOTURAN® II
The highest UV-sensitivity of raw FOTURAN® II is between 290 & 330 nm - Visible in the change of transmission slope