Product Variants of PYRAN® Platinum Fire-Rated Glass-Ceramics
PYRAN® Platinum
CHARACTERISTICS
With a thickness of 3/16" (5 mm), PYRAN® Platinum provides fire protection for up to 90 minutes with the required hose-stream test. Clear and colorless, the glass-ceramic also offers a smooth surface and distortion-free mirror finish, making it ideal for architectural applications.
YOUR ADVANTAGES
- Available in sheet size 51 x 99” – the largest in the industry.
- Weight: 2.6 lbs/ft²
- Can be used to construct insulated glazing units.
- Able to be lightly sandblasted or delivered with surface-applied opacity film without affecting the fire-rating.
- Produced without the hazardous heavy metals antimony and arsenic.
PYRAN® Platinum L
CHARACTERISTICS
With a thickness of 3/8” (9 mm), PYRAN® Platinum L provides fire protection for up to 90 minutes in windows and up to three hours in doors, both with the required hose stream test. Clear and colorless, the glass-ceramic also offers a smooth surface and distortion-free mirror finish, making it ideal for architectural applications.
YOUR ADVANTAGES
- Available in sheet size 51 x 99” – the largest in the industry.
- Transparent and wireless.
- Weight: 4.3 lbs/ft².
- Achieves the positive pressure test standard UL 10C.
- Can be used to construct insulated glazing units.
- Can be lightly sandblasted or delivered with surface-applied opacity film, without affecting the fire-rating.
- Produced without the hazardous heavy metals antimony and arsenic.
- Impact rating: ANSI Z97.1 (Class A) and CPSC 16CFR1201 (Cat. I and II).
PYRAN® Platinum F
CHARACTERISTICS
Designed to withstand impact as well as heat, hose stream and thermal shock, this clear, colorless glass-ceramic is fire-rated for up to 90 minutes in windows and up to 180 minutes in doors. Achieving the positive pressure test standard UL 10C, PYRAN® Platinum F can also be lightly sandblasted or delivered with surface-applied opacity film, without affecting its fire rating.
YOUR ADVANTAGES
- Available in sheet size 51 x 99” – the largest in the industry – and a thickness of 3/16” (5 mm).
- Weight: 2.6 lbs/ft².
- Microfloat production process results in a smooth surface and distortion-free mirror finish with surface-applied safety film.
- Clear and colorless without a distracting amber tint.
- Can be used to construct insulated glazing units.
- Produced without the hazardous heavy metals antimony and arsenic.
- Impact rating: ANSI Z97.1 and CPSC 16CFR1201 (Cat. I and II).
Daniel Poling