Passivation Glass
Finely tuned compositions for excellent component matching
Specifications
Passivation glasses are offered in a variety of individual specifications due to diversified glass systems. All passivation glasses are supplied as glass powder and available in different grain sizes.
Technology
Passivation glass powders are manufactured in two steps:
- The raw glass is first melted in specially designed aggregates.
- The glass ribbons are ground into fine powders of different grain size distribution.
Customers process our passivation glass powders in different ways. For the manufacturing of sintered glass diodes, a slurry of glass powder and deionized water is applied to the diode body before sintering it in a furnace. For wafer passivation, an organic suspension is applied by spinning, doctor blading, sedimentation, electrophoresis, or screen printing.