FLEXINITY®
Powerful, accurate and highly customizable
SCHOTT FLEXINITY® - Structured Glass Solutions
Standard structuring capabilities* | |
---|---|
Thickness range (depending on glass type) | 0.1 – 3.3 mm |
Format | Max. 600 mm in diameter (round, square) |
Layout | Through structures according to customer specifications |
Structuring radius | Down to 25 μm |
Minimum dimension of structure element | 100 μm |
Feature size tolerance | < 20 μm (equiv. ± 10 μm) |
Wall taper angle | 90 ° ± 0.5 ° |
Edge exclusion zone | ≥ 3 mm |
Position tolerance of features | < 20 μm (equiv. ± 10 μm) |
Bridge width between structure elements | Down to 100 μm |
*) limitations in feature design and demands deviating from these capabilities will be evaluated upon request
SCHOTT FLEXINITY® connect - Structured Glass Solutions
Structures | |
---|---|
Thickness range (depending on glass type) | ~ 0.2 – 1.1 mm |
Structuring radius |
Down to 50 µm |
Format | Max. 600 mm in diameter (round, square) |
Position tolerance | Down to ± 3 µm* |
Amount of holes | Up to 1000 holes per sec* |
Layouts | |
Structuring form | Round |
Position | Flexible |
Hole morphology | Straight |
Type | Through hole |
Material range** | |
D 263® T eco, BOROFLOAT® 33, SCHOTT® AF 35 G |
*) Depending on design
**) Other materials under evaluation
SCHOTT FLEXINITY® mini – Structured Glass Solutions
Standard structuring capabilities* | |
---|---|
Thickness range (depending on glass type) | 0.1 – 3.3 mm |
Format (Frame) | Max. 600 mm in diameter |
Size of detached parts | Down to 1mm |
Layout (outer contour of detached parts) | Round, rectangular, free shape |
Layout (holes) | Through structures according to customer specifications |
Outer contour & hole radius | Down to 25 μm |
Minimum dimensions of structure elements | 100 μm |
Feature size tolerance | < 20 μm (equiv. ± 10 μm) |
Position tolerance of features | < 20 μm (equiv. ± 10 μm) |
Frame size | ≥ 10 mm |
SCHOTT FLEXINITY® level – Structured Glass Solutions
Standard structuring capabilities* | |
---|---|
Glass Types | D263® T Eco, BOROFLOAT® 33 |
Thickness range (depending on glass type) | 0.6 – 3.3 mm |
Format | Max. 600 mm in diameter (round, square) |
Layout | Non-through structures according to customer specifications; can be combined with through structures* |
Structuring radius | Down to 25 μm |
Minimum dimension of structure element | 100 μm |
Feature size tolerance | < 20 μm (equiv. ± 10 μm) |
Wall taper angle | 90 ° ± 0.5 ° |
Edge exclusion zone | ≥ 3 mm |
Position tolerance of features | < 20 μm (equiv. ± 10 μm) |
Ridge width between structure elements | Down to 100 μm |
Specifications FLEXINITY® level | |
---|---|
Level Depth range, d1 | Min. 0.2 mm* |
Remaining Base Thickness, d0 | Min. 0.4 mm* |
Layout cavity | Round, rectangular, free shape |
Feature size tolerance (lateral) | < 20 μm (equiv. ± 10 μm) |
Position tolerance of features | < 20 μm (equiv. ± 10 μm) |
Level Depth tolerance | < 100 μm (equiv. ± 50 μm) |
Level Depth surface texture | Matte |
FLEXINITY® materials
SCHOTT FLEXINITY® is available as:
- D 263® T eco
- D 263® bio
- AF 32® eco
- MEMpax®
- BOROFLOAT®
To find out more, please see the related materials on the overview page.