Lithium Ion Battery Protectors

Surface mount SEFUSE® D6S battery fuses cut off circuits in the event of overcurrent and overcharging, helping to prevent fires caused by overheating, while SEREB® thermal battery protection switches interrupt current flow in the event of a device overheating, or when overcurrent causes abnormal heat levels. 

Features of SCHOTT Battery Protectors

SEFUSE® D6S battery fuses

SEFUSE® D6S battery fuses are surface mount devices, enabling thin and compact designs. SCHOTT offers product variations in accordance with requirements for different package sizes and rated current values. Our product line includes battery fuses compatible with up to 14 cells.

SEREB® thermal battery protection switches

SEREB® thermal battery protection switches are composed of elements using anti-corrosion materials known as 'bimetal'. In combination with its airtight construction, this material enables exceptional durability of the bimetal switch.

SEFUSE® D6S battery fuses product table

SCHOTT offers a wide range of battery fuses manufactured in accordance with varying package sizes and rated current.

 

Series Electrical Ratings Size (mm) Safety Standard
Rated
Current (A)
Rated
Voltage (Vdc)
Height Length Width
SCHOTT_DS_Series_D6SE_720_x_420_px.jpg D6SE series 30 80 1.70 9.50 5.00 UL/TÜV
45
60
SCHOTT_DS_Series_D6SA_720_x_420_px.jpg D6SA series 12 36 0.90 5.40 3.20 UL/TÜV
15
30 62
SCHOTT_DS_Series_D6SC_720_x_420_px.jpg D6SC series 12 36 0.85 4.00 3.00 UL/TÜV
15
22 62

 

 

 

SEFUSE® D6S battery fuses - Ratings

SEFUSE D6S Battery Fuse rating table_English

 

Dimension / Wiring Diagram

SEFUSE D6S Battery Fuse Dimension / Wiring Diagram_English

SEREB® thermal battery protection switch - Ratings

 

 
Part Number Action
Temperature
Internal
Resistance
Contact
Rating
Maximum
Interrupting
Currentet
Maximum
Interrupting
Volatage
Self Holding
Minimum
Voltage
Self Holding
Maximum
Current
UL  TÜV 

SB72X2

72 ± 5℃ 

 

≦8mΩ

 

 

DC10V/12A

 6000 Cycle

 

 

 

DC5V/40A
100 Cycle

 

 

 

DC28V/5A
100 Cycle

 

 

 

2V
(25℃)

 

 

 

150mA
(25℃)

 

 

E344840

 

 

R50251001

 

SB77X2 

77 ± 5℃ 

SB82X2 

82 ± 5℃

 SB85X2

85 ± 5℃ 

 

 

SEREB.png

Want to know more? Let’s talk

Whether you need more information, samples, a quote, or advice for a project, we would be delighted to talk to you.

Spojte se s námi
Man in glasses in business office on phone while working on laptop_605x350.jpg
!

Preview environment - pls. be aware that this page only displays the staged content and is not functional!